Bonding strengths to porcelain: An in vitro study of ultrasonic and conventional tooth preparation and etching
Journal article   Peer reviewed

Bonding strengths to porcelain: An in vitro study of ultrasonic and conventional tooth preparation and etching

David Chew, Vincent Bennani, John M Aarts, Nicholas Chandler, Andrew Gray and Bronwyn Lowe
Journal of Conservative Dentistry and Endodontics, Vol.22(1), pp.76-81
01/2019
Handle:
https://hdl.handle.net/10523/25828

Abstract

porcelain ultrasonic Bonding strengths
To compare the bond strength of porcelain to enamel and dentin preparations finished with either ultrasonic instruments or diamond burs, with or without acid etching. A total of 140 extracted bovine incisor teeth were divided into two groups, enamel and dentin. A split tooth model was employed: each tooth having a randomly allocated combination of diamond burs, ultrasonic instrument, etching, and no etching treatments on their labial surface. Lithium disilicate glass ceramic specimens were bonded to the prepared surfaces and tensile testing was carried out. Force was applied to failure, and linear mixed models were used to analyze the data. Etching increased the bond strength of the dentin samples by 7.63 MPa ( < 0.001). When bonding to dentin, ultrasonic instrument preparation produced a 2.88 MPa greater bond strength compared to burs ( < 0.001). Ultrasonic preparation produced greater bond strengths compared to rotary instruments. Etching improved the bond strength of all preparations, with enamel having consistently greater bonding values than dentin.